<?xml version="1.0" encoding="UTF-8"?><!DOCTYPE article  PUBLIC "-//NLM//DTD Journal Publishing DTD v3.0 20080202//EN" "http://dtd.nlm.nih.gov/publishing/3.0/journalpublishing3.dtd"><article xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink" dtd-version="3.0" xml:lang="en" article-type="research article"><front><journal-meta><journal-id journal-id-type="publisher-id">MP</journal-id><journal-title-group><journal-title>Modern  Physics</journal-title></journal-title-group><issn pub-type="epub">2161-0916</issn><publisher><publisher-name>Scientific Research Publishing</publisher-name></publisher></journal-meta><article-meta><article-id pub-id-type="doi">10.12677/MP.2017.71001</article-id><article-id pub-id-type="publisher-id">MP-19539</article-id><article-categories><subj-group subj-group-type="heading"><subject>MP20170100000_83346206.pdf</subject></subj-group><subj-group subj-group-type="Discipline-v2"><subject>数学与物理</subject></subj-group></article-categories><title-group><article-title>
 
 
  反钙钛矿结构镍基氮化物的研究进展
  Progress on the Studies of Antiperovskite Structure Nickel-Based Nitrides
 
</article-title></title-group><contrib-group><contrib contrib-type="author" xlink:type="simple"><name name-style="western"><surname>张</surname><given-names>敏</given-names></name><xref ref-type="aff" rid="aff1"><sup>1</sup></xref><xref ref-type="corresp" rid="cor1"><sup>*</sup></xref></contrib><contrib contrib-type="author" xlink:type="simple"><name name-style="western"><surname>宋</surname><given-names>婷婷</given-names></name><xref ref-type="aff" rid="aff1"><sup>1</sup></xref><xref ref-type="aff" rid="aff2"><sup>2</sup></xref></contrib></contrib-group><aff id="aff1"><addr-line>物理与空间科学学院，西华师范大学，四川 南充</addr-line></aff><aff id="aff2"><addr-line>null</addr-line></aff><author-notes><corresp id="cor1">* E-mail:<email>zmzmi_2005@163.com(张敏)</email>;</corresp></author-notes><pub-date pub-type="epub"><day>17</day><month>01</month><year>2017</year></pub-date><volume>07</volume><issue>01</issue><fpage>1</fpage><lpage>7</lpage><permissions><copyright-statement>&#169; Copyright  2014 by authors and Scientific Research Publishing Inc. </copyright-statement><copyright-year>2014</copyright-year><license><license-p>This work is licensed under the Creative Commons Attribution International License (CC BY). http://creativecommons.org/licenses/by/4.0/</license-p></license></permissions><abstract><p>
 
 
   
   反钙钛矿结构化合物的晶格结构与高温铜氧化物超导体中的钙钛矿结构单元相似，这类材料蕴含了丰富的物性，在超导、巨磁阻等领域有广阔的应用潜力。本文详细的介绍了反钙钛矿结构镍基氮化物的制备方法；总结了各项物理性质。 The crystal structure of anti-perovskite compounds is similar to the perovskite compounds structure unit of high temperature copper oxide superconductors. They have potential application in high temperature superconductivity and giant magnetoresistance due to their multiple physical properties. The preparation method of antiperovskite structure nickel-based nitrides was reviewed in this paper, and the various physical properties were summarized.
    
  
 
</p></abstract><kwd-group><kwd>反钙钛矿化合物，超导，镍基氮化物, Anti-Perovskite Compound</kwd><kwd> Superconductivity</kwd><kwd> Nickel-Based Nitrides</kwd></kwd-group></article-meta></front><body><sec id="s1"><title>反钙钛矿结构镍基氮化物的研究进展<sup> </sup></title><p>张敏，宋婷婷</p><p>物理与空间科学学院，西华师范大学，四川 南充</p><disp-formula id="hanspub.19539-formula1"><graphic xlink:href="http://html.hanspub.org/file/1-1260201x6_hanspub.png"  xlink:type="simple"/></disp-formula><p>收稿日期：2016年12月25日；录用日期：2017年1月14日；发布日期：2017年1月17日</p><disp-formula id="hanspub.19539-formula2"><graphic xlink:href="http://html.hanspub.org/file/1-1260201x7_hanspub.png"  xlink:type="simple"/></disp-formula></sec><sec id="s2"><title>摘 要</title><p>反钙钛矿结构化合物的晶格结构与高温铜氧化物超导体中的钙钛矿结构单元相似，这类材料蕴含了丰富的物性，在超导、巨磁阻等领域有广阔的应用潜力。本文详细的介绍了反钙钛矿结构镍基氮化物的制备方法；总结了各项物理性质。</p><p>关键词 :反钙钛矿化合物，超导，镍基氮化物</p><disp-formula id="hanspub.19539-formula3"><graphic xlink:href="http://html.hanspub.org/file/1-1260201x8_hanspub.png"  xlink:type="simple"/></disp-formula></sec><sec id="s3"><title>1. 引言</title><p>反钙钛矿结构化合物与钙钛矿化合物结构相似，反钙钛矿化合物的通式为XYM<sub>3</sub> [<xref ref-type="bibr" rid="hanspub.19539-ref1">1</xref>] ，其中X为主族元素或La系元素等；Y为B，C，N，O元素；M为碱金属元素，过渡族金属元素以及稀土族元素等。Y元素的位置是在由6个面心位置的M元素组成的八面体的中心，而在钙钛矿结构中，非金属元素Y和过渡族金属元素M交换位置 [<xref ref-type="bibr" rid="hanspub.19539-ref2">2</xref>] ，因此把XYM<sub>3</sub>称为反钙钛矿结构化合物。反钙钛矿结构化合物的物理性质丰富，如巨磁电阻 [<xref ref-type="bibr" rid="hanspub.19539-ref3">3</xref>] ，超导电性 [<xref ref-type="bibr" rid="hanspub.19539-ref4">4</xref>] ，负热膨胀 [<xref ref-type="bibr" rid="hanspub.19539-ref5">5</xref>] ，恒电阻率 [<xref ref-type="bibr" rid="hanspub.19539-ref6">6</xref>] 等，但是目前研究仍然较少。2001年Cava教授的课题组 [<xref ref-type="bibr" rid="hanspub.19539-ref7">7</xref>] 首次报道了MgCNi<sub>3</sub> (见图1)的反钙钛矿结构和超导性质。由于其含有高铁磁元素含量，结构却呈现超导性质，以MgCNi<sub>3</sub>代表的反钙钛矿镍基化合物迅速成为凝聚态和超导物理领域的研究热点。随后大量后续报道了用不同方法制备得到反钙钛矿镍基化合物样品，对其结构，输运性质，磁性，超导电性都进行了研究。本文详细介绍镍基氮化物材料。</p><p>镍基氮化物的式子可写为MNNi<sub>3</sub> (A = Zn, Cd, Mg, Al, Ga, In, Sn, Sb, Pd, Cu, Ag、Pt等)。实验制备出来的比较少，其中InNNi<sub>3</sub>和ZnNNi<sub>3</sub>研究较多，ZnNNi<sub>3</sub>是镍基氮化物里唯一发现的超导体，它们的制备都是利用镍粉和A金属的粉末研磨压片在NH<sub>3</sub>气体中烧结。大部分N化物为泡利顺磁体，呈金属行为。除此之外的物理化学性质几乎没有涉及。</p></sec><sec id="s4"><title>2. 超导体ZnNNi<sub>3</sub></title><p>Uehara等 [<xref ref-type="bibr" rid="hanspub.19539-ref8">8</xref>] 采用固相法合成了为ZnNNi<sub>3</sub>的样品(图2)。采用原料为Zn粉、Ni粉，这些粉末按名义组分Zn<sub>1.05</sub>Ni<sub>3</sub>研磨压片，然后在NH<sub>3</sub>气氛环境下烧结。过量的Zn是为了补充Zn蒸发造成了缺失。升温到400℃后保温3小时后冷却后研磨压片，再升温到520℃保温15小时冷却后再次研磨压片，最后在600℃保温5 h。NH<sub>3</sub>气会分解成氢气和氮气，高温下氮气就会进入Zn<sub>1.05</sub>Ni<sub>3</sub>。</p><p>ZnNNi<sub>3</sub> [<xref ref-type="bibr" rid="hanspub.19539-ref9">9</xref>] 为立方结构，空间群Pm3m，六个Ni原子处在面心位置和体心的N原子构成Ni<sub>6</sub>N八面体。晶格常数a = 3.756 &#197;，与ZnCNi<sub>3</sub>3.772 [<xref ref-type="bibr" rid="hanspub.19539-ref10">10</xref>] 接近。a (ZnCNi<sub>3 </sub>= 3.772 &#197;) &gt; a (ZnNNi<sub>3</sub>)，而结果可以解释为碳原子和氮原子的原子半径比为：R(C) = 0.77 &#197; &gt; R(N) = 0.71 &#197;。</p><p>Shein等 [<xref ref-type="bibr" rid="hanspub.19539-ref10">10</xref>] 和Okoye等 [<xref ref-type="bibr" rid="hanspub.19539-ref11">11</xref>] 研究了ZnNNi<sub>3</sub>的电子结构，比热，弹性等，Okoye等 [<xref ref-type="bibr" rid="hanspub.19539-ref11">11</xref>] 通过对能带结构的研究，得出ZnNNi<sub>3</sub>呈金属性。Xu等 [<xref ref-type="bibr" rid="hanspub.19539-ref12">12</xref>] 认为ZnNNi<sub>3</sub>和ZnCNi<sub>3</sub>的电子结构相似，但N2p的能量比C2p更低。费米能级处电子能态密度主要由Ni3d和N2p杂化提供。其他参数见表1。根据 [<xref ref-type="bibr" rid="hanspub.19539-ref10">10</xref>] [<xref ref-type="bibr" rid="hanspub.19539-ref13">13</xref>] 中的计算，体积模量B &gt; 剪切模量G，这个结果暗示这种的机械稳定性取决剪切模量G。根据文献 [<xref ref-type="bibr" rid="hanspub.19539-ref14">14</xref>] 中的理论，若B/G的比值小于1.75，材料具有脆性，若B/G的比值大于1.75，材料具有韧性。ZnNNi<sub>3</sub>的B/G值为6.26，MgCNi<sub>3</sub>的B/G值为4，这意味着ZnNNi<sub>3</sub>是一种比MgCNi<sub>3</sub>更具有韧性的材料。</p><p>体积模量B(ZnNNi<sub>3</sub>) &lt; B(ZnCNi<sub>3</sub>)，与晶格大导致体积模量小的规律符合的很好。从表1中可看到费米能级N(E<sub>F</sub>) (ZnNNi<sub>3</sub>) = 2.813 states/eV cell，和N(E<sub>F</sub>) MgCNi<sub>3</sub> = 5.280 states/eV cell相比，前者小于后者，Shein等 [<xref ref-type="bibr" rid="hanspub.19539-ref10">10</xref>] [<xref ref-type="bibr" rid="hanspub.19539-ref13">13</xref>] 认为根据N(E<sub>F</sub>)值较大，有利于实现超导这一推论，这也可以解释ZnNNi<sub>3</sub>的T<sub>c</sub> (3 K)小于MgCNi<sub>3</sub>的T<sub>c</sub> (8 K)。而Okoye等 [<xref ref-type="bibr" rid="hanspub.19539-ref11">11</xref>] 认为ZnNNi<sub>3</sub>的N(E<sub>F</sub>)约为ZnCNi<sub>3</sub>的一半，ZnNNi<sub>3</sub>的T<sub>c</sub>为3 K，ZnCNi<sub>3</sub></p><p>图1. (a)超导体MgCNi<sub>3</sub>的反钙钛矿结构，（b) MgCNi<sub>3</sub>在290 K - 5 K的电阻率温度曲线，超导转变温度为8.5 K [<xref ref-type="bibr" rid="hanspub.19539-ref7">7</xref>]</p><p>图2. ZnNNi<sub>3</sub> (x = 0.95, 1.00, 1.10)的XRD谱 [<xref ref-type="bibr" rid="hanspub.19539-ref8">8</xref>]</p><table-wrap id="table1" ><label><xref ref-type="table" rid="table1">Table 1</xref></label><caption><title> The comparison of ZnNNi3 and ZnCNi</title></caption><table><tbody><thead><tr><th align="center" valign="middle" >Parameters</th><th align="center" valign="middle"  colspan="3"  >ZnNNi<sub>3</sub></th><th align="center" valign="middle"  colspan="3"  >ZnCNi<sub>3 </sub></th></tr></thead><tr><td align="center" valign="middle" >ɑ (&#197;)</td><td align="center" valign="middle" >3.769</td><td align="center" valign="middle" >3.719</td><td align="center" valign="middle" >3.763</td><td align="center" valign="middle" >3.772</td><td align="center" valign="middle" >3.728</td><td align="center" valign="middle" >3.770</td></tr><tr><td align="center" valign="middle" >C11 (GPa)</td><td align="center" valign="middle" >364.20</td><td align="center" valign="middle" >394.57</td><td align="center" valign="middle" >351.69</td><td align="center" valign="middle" >319.53</td><td align="center" valign="middle" >400.57</td><td align="center" valign="middle" >356.04</td></tr><tr><td align="center" valign="middle" >C12 (GPa)</td><td align="center" valign="middle" >124.9</td><td align="center" valign="middle" >140.28</td><td align="center" valign="middle" >127.97</td><td align="center" valign="middle" >105.72</td><td align="center" valign="middle" >131.64</td><td align="center" valign="middle" >122.42</td></tr><tr><td align="center" valign="middle" >C44 (GPa) = G</td><td align="center" valign="middle" >32.69</td><td align="center" valign="middle" >55.39</td><td align="center" valign="middle" >56.34</td><td align="center" valign="middle" >39.42</td><td align="center" valign="middle" >32.35</td><td align="center" valign="middle" >44.60</td></tr><tr><td align="center" valign="middle" >B (GPa)</td><td align="center" valign="middle" >204.66</td><td align="center" valign="middle" >225.04</td><td align="center" valign="middle" >202.54</td><td align="center" valign="middle" >176.99</td><td align="center" valign="middle" >221.28</td><td align="center" valign="middle" >200.29</td></tr><tr><td align="center" valign="middle" >β</td><td align="center" valign="middle" >0.004886</td><td align="center" valign="middle" ></td><td align="center" valign="middle" ></td><td align="center" valign="middle" >0.005650</td><td align="center" valign="middle" ></td><td align="center" valign="middle" ></td></tr><tr><td align="center" valign="middle" >N(E<sub>F</sub>) (total) states/eV cell</td><td align="center" valign="middle" >2.813</td><td align="center" valign="middle" ></td><td align="center" valign="middle" ></td><td align="center" valign="middle" >4.341</td><td align="center" valign="middle" ></td><td align="center" valign="middle" ></td></tr><tr><td align="center" valign="middle" >Θ<sub>D</sub> (K)</td><td align="center" valign="middle" ></td><td align="center" valign="middle" >276.47</td><td align="center" valign="middle" >271.57</td><td align="center" valign="middle" ></td><td align="center" valign="middle" >244.64</td><td align="center" valign="middle" >258.27</td></tr><tr><td align="center" valign="middle" ><inline-formula><inline-graphic xlink:href="http://html.hanspub.org/file/1-1260201x12_hanspub.png" xlink:type="simple"/></inline-formula>mJ/molf.u. K<sup>2</sup></td><td align="center" valign="middle" >6.631 6.5 [<xref ref-type="bibr" rid="hanspub.19539-ref12">12</xref>]</td><td align="center" valign="middle" ></td><td align="center" valign="middle" ></td><td align="center" valign="middle" >10.23 12.6 [<xref ref-type="bibr" rid="hanspub.19539-ref12">12</xref>]</td><td align="center" valign="middle" ></td><td align="center" valign="middle" ></td></tr><tr><td align="center" valign="middle" ><inline-formula><inline-graphic xlink:href="http://html.hanspub.org/file/1-1260201x13_hanspub.png" xlink:type="simple"/></inline-formula>10<sup>−4</sup> mu/mol</td><td align="center" valign="middle" >0.905 0.89 [<xref ref-type="bibr" rid="hanspub.19539-ref12">12</xref>]</td><td align="center" valign="middle" ></td><td align="center" valign="middle" ></td><td align="center" valign="middle" >1.40 1.72 [<xref ref-type="bibr" rid="hanspub.19539-ref12">12</xref>]</td><td align="center" valign="middle" ></td><td align="center" valign="middle" ></td></tr><tr><td align="center" valign="middle" >Ref</td><td align="center" valign="middle" >[<xref ref-type="bibr" rid="hanspub.19539-ref10">10</xref>]</td><td align="center" valign="middle"  colspan="2"  >[<xref ref-type="bibr" rid="hanspub.19539-ref11">11</xref>]</td><td align="center" valign="middle" >[<xref ref-type="bibr" rid="hanspub.19539-ref10">10</xref>]</td><td align="center" valign="middle"  colspan="2"  >[<xref ref-type="bibr" rid="hanspub.19539-ref11">11</xref>]</td></tr></tbody></table></table-wrap><p>表1. ZnNNi<sub>3</sub>和ZnCNi<sub>3</sub>的比较</p><p>在2 K以下未见超导迹象，这暗示了费米能级处的电子能态密度的减少也导致了相应的反钙钛矿氮化物超导体的高的T<sub>c</sub>。</p><p>从图3可以看出ZnNNi<sub>3</sub>在3 K发生超导转变。根据文献报道，作者列举了超导体ZnNNi<sub>3</sub>的一些参数，见表1。</p><p>ZnNi<sub>3</sub>为立方结构，空间群Pm3m，六个Ni原子处在面心位置，和ZnNNi<sub>3</sub>，ZnCNi<sub>3</sub>相比，体心位置无N或C，晶格常数为3.552，比ZnNNi3，ZnCNi<sub>3</sub>小。Xu [<xref ref-type="bibr" rid="hanspub.19539-ref12">12</xref>] 等计算得出ZnNi<sub>3</sub>的低温电子比热系数<inline-formula><inline-graphic xlink:href="http://html.hanspub.org/file/1-1260201x14_hanspub.png" xlink:type="simple"/></inline-formula>= 22 mJ/molf.u. K<sup>2</sup>，<inline-formula><inline-graphic xlink:href="http://html.hanspub.org/file/1-1260201x15_hanspub.png" xlink:type="simple"/></inline-formula> = 10<sup>−4</sup> emu/mol，<inline-formula><inline-graphic xlink:href="http://html.hanspub.org/file/1-1260201x16_hanspub.png" xlink:type="simple"/></inline-formula>和<inline-formula><inline-graphic xlink:href="http://html.hanspub.org/file/1-1260201x17_hanspub.png" xlink:type="simple"/></inline-formula>的值遵循ZnNNi<sub>3</sub> &lt; ZnCNi<sub>3</sub> &lt; ZnNi<sub>3</sub>的排序。由Stoner parameter (S)<inline-formula><inline-graphic xlink:href="http://html.hanspub.org/file/1-1260201x18_hanspub.png" xlink:type="simple"/></inline-formula>知<inline-formula><inline-graphic xlink:href="http://html.hanspub.org/file/1-1260201x19_hanspub.png" xlink:type="simple"/></inline-formula>为3.7大于1 (stoner判据<inline-formula><inline-graphic xlink:href="http://html.hanspub.org/file/1-1260201x20_hanspub.png" xlink:type="simple"/></inline-formula>&gt; 1为形成铁磁序)，则ZnNi<sub>3</sub>呈现铁磁性。由此推测ZnNNi<sub>3</sub>和ZnCNi<sub>3</sub>是无磁性材料，而当它们N/C缺位时，就表现出了磁性。</p><p>Li等 [<xref ref-type="bibr" rid="hanspub.19539-ref15">15</xref>] 采用第一性原理计算了MNNi<sub>3</sub>系列的化合物，其中M = Zn、Mg、Cd，得到晶格常数的大小排列为<inline-formula><inline-graphic xlink:href="http://html.hanspub.org/file/1-1260201x21_hanspub.png" xlink:type="simple"/></inline-formula>a(ZnNNi<sub>3</sub>) &lt; a (MgNNi<sub>3</sub>) &lt; a(CdNNi<sub>3</sub>)，符合晶格大导致体积模量小的规律。费米能级处电子能态密度主要由Ni 3d电子和N2p之间电子的杂化提供。虽然元素M在材料中对N(E<sub>F</sub>)的贡献很小，但M可能导致了费米能级附近的能带发生微小的转移，从而影响N(E<sub>F</sub>)的值。不同的M元素，改变的电声子对不同，使得ZnNNi<sub>3</sub>的N(E<sub>F</sub>)值为这3种化合物中最大的。但MgNNi<sub>3</sub>、CdNNi<sub>3</sub>是否具有超导性，ZnNNi<sub>3</sub>的N(E<sub>F</sub>)值最大是否导致其再这3种化合物中T<sub>c</sub>最大还未见报道。</p></sec><sec id="s5"><title>3. InNNi<sub>3</sub></title><p>Uehara等 [<xref ref-type="bibr" rid="hanspub.19539-ref16">16</xref>] 用固相反应法制备了InNNi<sub>3</sub>，样品制备使用原料为In粉、Ni粉，按名义组分，InNi<sub>3</sub>研磨压片置于NH<sub>3</sub>气中烧结，500℃保温5 h，冷却后研磨压片，再在NH<sub>3</sub>气中升温到600℃保温5 h。Cao等 [<xref ref-type="bibr" rid="hanspub.19539-ref17">17</xref>] 等也使用固相法，把In:Ni = 1:3的InNi<sub>3</sub>片于NH<sub>3</sub>气中升温600℃~650℃保温10 h (图4)。</p><p>InNNi<sub>3</sub>为立方结构，空间群Pm3m，晶格常数<inline-formula><inline-graphic xlink:href="http://html.hanspub.org/file/1-1260201x22_hanspub.png" xlink:type="simple"/></inline-formula>= 3.854 &#197;。由电输运测量电阻率和温度的关系ρ(T)曲线呈现金属性行为。70 K以上为费米液体行为(<inline-formula><inline-graphic xlink:href="http://html.hanspub.org/file/1-1260201x23_hanspub.png" xlink:type="simple"/></inline-formula>)，70 K以下电阻率和温度关系呈线性(<inline-formula><inline-graphic xlink:href="http://html.hanspub.org/file/1-1260201x24_hanspub.png" xlink:type="simple"/></inline-formula>)，偏离费米液体行为。零场冷(ZFC)和场冷(FC)测量结果显示InNNi<sub>3</sub>为顺磁体(图5)。</p><p>Hou [<xref ref-type="bibr" rid="hanspub.19539-ref18">18</xref>] 研究了InNNi<sub>3</sub>和相似结构的化合物InNCo<sub>3</sub>的晶格常数，弹性，电子结构，参数见表2。</p><p>图3. (a) ZnNNi<sub>3</sub>的电阻率温度曲线，插图显示其在1.8 K - 300 K的电阻率和温度的关系，(b) ZnNNi<sub>3</sub>在10 Oe磁场下测试的1.8 K - 5 K的场冷和零场冷曲线 [<xref ref-type="bibr" rid="hanspub.19539-ref8">8</xref>]</p><p>图4. InNNi<sub>3</sub>的XRD谱 [<xref ref-type="bibr" rid="hanspub.19539-ref17">17</xref>]</p><p>图5. IINNi<sub>3</sub>在20 Oe磁场下测试的场冷和零场冷曲线 [<xref ref-type="bibr" rid="hanspub.19539-ref17">17</xref>]</p><table-wrap id="table2" ><label><xref ref-type="table" rid="table2">Table 2</xref></label><caption><title> The relevant parameters of InNNi3 and InNCo</title></caption><table><tbody><thead><tr><th align="center" valign="middle"  rowspan="2"  ></th><th align="center" valign="middle" >InNNi<sub>3</sub></th><th align="center" valign="middle" ></th><th align="center" valign="middle" >InNCo<sub>3</sub></th><th align="center" valign="middle" ></th></tr></thead><tr><td align="center" valign="middle" >LDA</td><td align="center" valign="middle" >GGA</td><td align="center" valign="middle" >LDA</td><td align="center" valign="middle" >GGA</td></tr><tr><td align="center" valign="middle" ><inline-formula><inline-graphic xlink:href="http://html.hanspub.org/file/1-1260201x28_hanspub.png" xlink:type="simple"/></inline-formula></td><td align="center" valign="middle" >3.74</td><td align="center" valign="middle" >3.882</td><td align="center" valign="middle" >3.744</td><td align="center" valign="middle" >3.753</td></tr><tr><td align="center" valign="middle" >B</td><td align="center" valign="middle" >226.92</td><td align="center" valign="middle" >279.93</td><td align="center" valign="middle" >255.78</td><td align="center" valign="middle" >243.06</td></tr><tr><td align="center" valign="middle" >C<sub>11</sub></td><td align="center" valign="middle" >356.77</td><td align="center" valign="middle" >274.08</td><td align="center" valign="middle" >389.11</td><td align="center" valign="middle" >317.54</td></tr><tr><td align="center" valign="middle" >C<sub>12</sub></td><td align="center" valign="middle" >164.23</td><td align="center" valign="middle" >131.20</td><td align="center" valign="middle" >171.12</td><td align="center" valign="middle" >126.76</td></tr><tr><td align="center" valign="middle" >C<sub>44</sub></td><td align="center" valign="middle" >69.06</td><td align="center" valign="middle" >60.01</td><td align="center" valign="middle" >102.55</td><td align="center" valign="middle" >94.98</td></tr><tr><td align="center" valign="middle" >G</td><td align="center" valign="middle" >79.24</td><td align="center" valign="middle" >64.35</td><td align="center" valign="middle" >105.08</td><td align="center" valign="middle" >95.14</td></tr><tr><td align="center" valign="middle" ><inline-formula><inline-graphic xlink:href="http://html.hanspub.org/file/1-1260201x29_hanspub.png" xlink:type="simple"/></inline-formula></td><td align="center" valign="middle" >0.344</td><td align="center" valign="middle" >0.339</td><td align="center" valign="middle" >0.311</td><td align="center" valign="middle" >0.286</td></tr><tr><td align="center" valign="middle" >B/G</td><td align="center" valign="middle" >2.895</td><td align="center" valign="middle" >2.779</td><td align="center" valign="middle" >2.320</td><td align="center" valign="middle" >2.001</td></tr><tr><td align="center" valign="middle" >Ref</td><td align="center" valign="middle"  colspan="4"  >[<xref ref-type="bibr" rid="hanspub.19539-ref18">18</xref>]</td></tr></tbody></table></table-wrap><p>表2. InNNi<sub>3</sub>和InNCo<sub>3</sub>的相关参数</p><p>晶格常数大小排列a(InNNi<sub>3</sub>) &gt; a(InCNi<sub>3</sub>) &gt; a(InNCo<sub>3</sub>) &gt; a(ZnNNi<sub>3</sub>)，体积模量排列B(InNNi<sub>3</sub>) &lt; B(InCNi<sub>3</sub>) &lt; B(InNCo<sub>3</sub>) &lt; B(ZnNNi<sub>3</sub>)，符合晶格大导致体积模量小的规律。剪切模量G(ZnNNi<sub>3</sub>和InNNi<sub>3</sub>) &lt; G(InCNi<sub>3</sub>) &lt; G(InNCo<sub>3</sub>)，与B排列相反。根据B/G比值，ZnNNi<sub>3</sub>、InNNi<sub>3</sub>、InCNi<sub>3</sub>和InNCo<sub>3</sub>都是韧性材料。费米能级处电子能态密度主要由Ni3d和N2p杂化提供。</p></sec><sec id="s6"><title>4. 其他镍基N化物MNNi<sub>3</sub> (M = Al、Ga、Sn、Sb、Pd、Cu、Ag、Pt)</title><p>MNNi<sub>3</sub>体系的晶格常数的计算采用公式：<inline-formula><inline-graphic xlink:href="http://html.hanspub.org/file/1-1260201x30_hanspub.png" xlink:type="simple"/></inline-formula> = 2.14R (Ni-0.072R<sub>M</sub> (M = Al、Ga、In、Sn、Sb、Pd、Cu、Ag、Pt等) + 1.228 [<xref ref-type="bibr" rid="hanspub.19539-ref19">19</xref>] ，从CuNNi<sub>3</sub> = 3.910 &#197;到SbNNi<sub>3</sub> = 3.942 &#197;，晶格常数的大小和M原子半径相关。如<inline-formula><inline-graphic xlink:href="http://html.hanspub.org/file/1-1260201x31_hanspub.png" xlink:type="simple"/></inline-formula>(AlNNi3) = 3.777&#197;~<inline-formula><inline-graphic xlink:href="http://html.hanspub.org/file/1-1260201x32_hanspub.png" xlink:type="simple"/></inline-formula> (GaNNi<sub>3</sub>) = 3.778&#197; &lt; <inline-formula><inline-graphic xlink:href="http://html.hanspub.org/file/1-1260201x33_hanspub.png" xlink:type="simple"/></inline-formula> (InNNi<sub>3</sub>) [<xref ref-type="bibr" rid="hanspub.19539-ref20">20</xref>] ，用原子半径来解释，R(Al) = 1.43 &#197;~R(Ga) = 1.39 &#197; &lt; R(In) = 1.66 &#197;。根据 [<xref ref-type="bibr" rid="hanspub.19539-ref19">19</xref>] 密度大小如下，<inline-formula><inline-graphic xlink:href="http://html.hanspub.org/file/1-1260201x34_hanspub.png" xlink:type="simple"/></inline-formula> (AlNNi<sub>3</sub>) = 6.689 g/cm<sup>3</sup>，<inline-formula><inline-graphic xlink:href="http://html.hanspub.org/file/1-1260201x35_hanspub.png" xlink:type="simple"/></inline-formula> (GaNNi<sub>3</sub>) = 7.936 g/cm<sup>3</sup>，<inline-formula><inline-graphic xlink:href="http://html.hanspub.org/file/1-1260201x36_hanspub.png" xlink:type="simple"/></inline-formula> (InNNi<sub>3</sub>) = 8.661 g/cm<sup>3</sup>。密度随M原子质量的增加而增加。</p><p>体积模量B(InNNi<sub>3</sub>) &lt; B(GaNNi<sub>3</sub>) &lt; B(AlNNi<sub>3</sub>)，和B~1/V符合的很好。最大的体积模量(最小的可压缩量)是PtNNi<sub>3</sub>。杨氏模量Y是描述固体材料抵抗形变能力的物理量，最大的杨氏模量为InNNi<sub>3</sub>和MgNNi<sub>3</sub>，最小的是SnNNi<sub>3</sub>，说明这类材料当中InNNi<sub>3</sub>硬度最大。SnNNi<sub>3</sub>最软。</p><p>对于MNNi<sub>3</sub> (M = Al、Ga、Sn、Sb、Cu、Ag、Pt)，B &gt; <inline-formula><inline-graphic xlink:href="http://html.hanspub.org/file/1-1260201x37_hanspub.png" xlink:type="simple"/></inline-formula> &gt; G，(<inline-formula><inline-graphic xlink:href="http://html.hanspub.org/file/1-1260201x38_hanspub.png" xlink:type="simple"/></inline-formula>为正方剪切模量)这意味着决定材料机械稳定性的参数是剪切模量G，对于InNNi<sub>3</sub>和PdNNi<sub>3</sub>，B &gt; G &gt;<inline-formula><inline-graphic xlink:href="http://html.hanspub.org/file/1-1260201x39_hanspub.png" xlink:type="simple"/></inline-formula>，这意味着决定这种材料机械稳定性的参数是<inline-formula><inline-graphic xlink:href="http://html.hanspub.org/file/1-1260201x40_hanspub.png" xlink:type="simple"/></inline-formula>。</p><p>脆性材料的泊松比比较小，韧性材料的泊松比为0.33左右。由此这类材料为韧性材料。根据B/G比值，大部分MNNi<sub>3</sub>物质都是韧性材料，除了InNNi<sub>3</sub>和MgNNi<sub>3</sub>处于脆性材料和韧性材料之间 [<xref ref-type="bibr" rid="hanspub.19539-ref20">20</xref>] ，和文献 [<xref ref-type="bibr" rid="hanspub.19539-ref18">18</xref>] 的结论不同(表3)。</p></sec><sec id="s7"><title>5. 结论</title><p>反钙钛矿镍基氮化物的报道还较少，样品制备工艺和物性研究有待于进一步深入。但由于反钙钛矿镍基化合物为三元化合物并且熔点高，因此目前获得的样品大部分为多晶，且相不纯。后期的研究应该致力探索制备单晶以减少物性测量误差，从而获得准确的物性。</p><table-wrap id="table3" ><label><xref ref-type="table" rid="table3">Table 3</xref></label><caption><title> Parameters of compounds and the related reference</title></caption><table><tbody><thead><tr><th align="center" valign="middle" >Phase parameters</th><th align="center" valign="middle" >AlNNi<sub>3</sub></th><th align="center" valign="middle" >GaNNi<sub>3</sub></th><th align="center" valign="middle"  colspan="2"  >MgNNi<sub>3</sub></th><th align="center" valign="middle" >SnNNi<sub>3</sub></th><th align="center" valign="middle" >SbNNi<sub>3</sub></th><th align="center" valign="middle" >PdNNi<sub>3</sub></th><th align="center" valign="middle" >PtNNi<sub>3</sub></th><th align="center" valign="middle" >CuNNi<sub>3</sub></th><th align="center" valign="middle" >AgNNi<sub>3</sub></th></tr></thead><tr><td align="center" valign="middle" ><inline-formula><inline-graphic xlink:href="http://html.hanspub.org/file/1-1260201x41_hanspub.png" xlink:type="simple"/></inline-formula>(&#197;)</td><td align="center" valign="middle" >3.777</td><td align="center" valign="middle" >3.788</td><td align="center" valign="middle"  colspan="2"  >3.815</td><td align="center" valign="middle" >3.910</td><td align="center" valign="middle" >3.942</td><td align="center" valign="middle" >3.803</td><td align="center" valign="middle" >3.809</td><td align="center" valign="middle" >3.745</td><td align="center" valign="middle" >3.832</td></tr><tr><td align="center" valign="middle" >B</td><td align="center" valign="middle" >207.9</td><td align="center" valign="middle" >201.8</td><td align="center" valign="middle"  colspan="2"  >179.1</td><td align="center" valign="middle" >182.3</td><td align="center" valign="middle" ></td><td align="center" valign="middle" >212.1</td><td align="center" valign="middle" >237.4</td><td align="center" valign="middle" >213.6</td><td align="center" valign="middle" >193.7</td></tr><tr><td align="center" valign="middle" >C11</td><td align="center" valign="middle" >431.4</td><td align="center" valign="middle" >336.8</td><td align="center" valign="middle"  colspan="2"  >319.9</td><td align="center" valign="middle" >239.9</td><td align="center" valign="middle" >226.7</td><td align="center" valign="middle" >313.3</td><td align="center" valign="middle" >316.9</td><td align="center" valign="middle" >396.9</td><td align="center" valign="middle" >321.1</td></tr><tr><td align="center" valign="middle" >C12</td><td align="center" valign="middle" >96.1</td><td align="center" valign="middle" >134.3</td><td align="center" valign="middle"  colspan="2"  >108.6</td><td align="center" valign="middle" >153.5</td><td align="center" valign="middle" >154.3</td><td align="center" valign="middle" >161.5</td><td align="center" valign="middle" >197.7</td><td align="center" valign="middle" >121.9</td><td align="center" valign="middle" >130.0</td></tr><tr><td align="center" valign="middle" >C44</td><td align="center" valign="middle" >48.0</td><td align="center" valign="middle" >34.9</td><td align="center" valign="middle"  colspan="2"  >96.9</td><td align="center" valign="middle" >2.2</td><td align="center" valign="middle" >8.6</td><td align="center" valign="middle" >81.1</td><td align="center" valign="middle" >50.5</td><td align="center" valign="middle" >7.8</td><td align="center" valign="middle" >48.9</td></tr><tr><td align="center" valign="middle" >G</td><td align="center" valign="middle" >81.6</td><td align="center" valign="middle" >54.4</td><td align="center" valign="middle"  colspan="2"  >100.3</td><td align="center" valign="middle" >11.1</td><td align="center" valign="middle" ></td><td align="center" valign="middle" >79.0</td><td align="center" valign="middle" >54</td><td align="center" valign="middle" >36.1</td><td align="center" valign="middle" >64.1</td></tr><tr><td align="center" valign="middle" ><inline-formula><inline-graphic xlink:href="http://html.hanspub.org/file/1-1260201x42_hanspub.png" xlink:type="simple"/></inline-formula></td><td align="center" valign="middle" ></td><td align="center" valign="middle" ></td><td align="center" valign="middle"  colspan="2"  >105.6</td><td align="center" valign="middle" >43.2</td><td align="center" valign="middle" ></td><td align="center" valign="middle" >75.9</td><td align="center" valign="middle" >59.6</td><td align="center" valign="middle" >137.5</td><td align="center" valign="middle" >95.5</td></tr><tr><td align="center" valign="middle" >Y</td><td align="center" valign="middle" >216.5</td><td align="center" valign="middle" >149.7</td><td align="center" valign="middle"  colspan="2"  >253.6</td><td align="center" valign="middle" >32.6</td><td align="center" valign="middle" ></td><td align="center" valign="middle" >210.8</td><td align="center" valign="middle" >150.5</td><td align="center" valign="middle" >102.6</td><td align="center" valign="middle" >173.3</td></tr><tr><td align="center" valign="middle" ><inline-formula><inline-graphic xlink:href="http://html.hanspub.org/file/1-1260201x43_hanspub.png" xlink:type="simple"/></inline-formula></td><td align="center" valign="middle" >0.327</td><td align="center" valign="middle" >0.376</td><td align="center" valign="middle"  colspan="2"  >0.264</td><td align="center" valign="middle" >0.470</td><td align="center" valign="middle" ></td><td align="center" valign="middle" >0.334</td><td align="center" valign="middle" >0.394</td><td align="center" valign="middle" >0.420</td><td align="center" valign="middle" >0.351</td></tr><tr><td align="center" valign="middle" >B/G</td><td align="center" valign="middle" >0.392</td><td align="center" valign="middle" >0.270</td><td align="center" valign="middle"  colspan="2"  >1.785</td><td align="center" valign="middle" >16.393</td><td align="center" valign="middle" ></td><td align="center" valign="middle" >2.688</td><td align="center" valign="middle" >4.405</td><td align="center" valign="middle" >5.917</td><td align="center" valign="middle" >3.0211</td></tr><tr><td align="center" valign="middle" >Ref</td><td align="center" valign="middle"  colspan="3"  >[<xref ref-type="bibr" rid="hanspub.19539-ref20">20</xref>]</td><td align="center" valign="middle"  colspan="5"  >[<xref ref-type="bibr" rid="hanspub.19539-ref14">14</xref>]</td><td align="center" valign="middle" ></td><td align="center" valign="middle" ></td></tr><tr><td align="center" valign="middle" ></td><td align="center" valign="middle" ></td><td align="center" valign="middle" ></td><td align="center" valign="middle" ></td><td align="center" valign="middle" ></td><td align="center" valign="middle" ></td><td align="center" valign="middle" ></td><td align="center" valign="middle" ></td><td align="center" valign="middle" ></td><td align="center" valign="middle" ></td><td align="center" valign="middle" ></td></tr></tbody></table></table-wrap><p>表3. 化合物参数及相关文献</p></sec><sec id="s8"><title>基金项目</title><p>四川省科技厅应用基础研究(项目号2014JY0133)；西华师范大学博士科研启动基金(项目号412577)。</p></sec><sec id="s9"><title>文章引用</title><p>张 敏,宋婷婷. 反钙钛矿结构镍基氮化物的研究进展 Progress on the Studies of Antiperovskite Structure Nickel-Based Nitrides[J]. 现代物理, 2017, 07(01): 1-7. http://dx.doi.org/10.12677/MP.2017.71001</p></sec><sec id="s10"><title>参考文献 (References)</title></sec></body><back><ref-list><title>References</title><ref id="hanspub.19539-ref1"><label>1</label><mixed-citation publication-type="other" xlink:type="simple">童鹏. 反钙钛矿结构镍基化合物研究[D]: [博士学位论文]. 合肥: 中国科学院研究生院(合肥物质科学研究院), 2007.</mixed-citation></ref><ref id="hanspub.19539-ref2"><label>2</label><mixed-citation publication-type="other" xlink:type="simple">刘光华. 稀土材料与应用技术[M]. 北京: 化学工业出版社, 2005.</mixed-citation></ref><ref id="hanspub.19539-ref3"><label>3</label><mixed-citation publication-type="other" xlink:type="simple">Kim, W.S., Chi, E.O, Kim, J.C., et al. (2001) Close Correlation among Lattice, Spin, and Charge in the Manganese-Based Antiperovskite Material. Solid State Communications, 119, 507-510.  
https://doi.org/10.1016/S0038-1098(01)00279-4</mixed-citation></ref><ref id="hanspub.19539-ref4"><label>4</label><mixed-citation publication-type="other" xlink:type="simple">Shein, I.R. and Ivanovskii, A.L. (2008) Electronic and Elastic Properties of Non-Oxide Anti-Perovskites from First Principles: Superconducting CdCNi3 in Comparison with Magnetic In CNi3. Physical Review B, 77, 104101.  
https://doi.org/10.1103/PhysRevB.77.104101</mixed-citation></ref><ref id="hanspub.19539-ref5"><label>5</label><mixed-citation publication-type="other" xlink:type="simple">Takenaka, K. and Takagi, H. (2005) Giant Negative Thermal Expansion in Ge-Doped Anti-Perovskite Manganese Nitrides. Applied Physics Letters, 87, 1902. https://doi.org/10.1063/1.2147726</mixed-citation></ref><ref id="hanspub.19539-ref6"><label>6</label><mixed-citation publication-type="other" xlink:type="simple">Chi, E.O., Kim, W.S. and Hur, N.H. (2001) Nearly Zero Temperature Coefficient of Resistivity in Antiperovskite Compound CuNMn3. Solid State Communications, 120, 307-310. https://doi.org/10.1016/S0038-1098(01)00395-7</mixed-citation></ref><ref id="hanspub.19539-ref7"><label>7</label><mixed-citation publication-type="other" xlink:type="simple">He, T., Huang, Q., Ramirez, A.P., et al. (2001) Superconductivity in the Non-Oxide Perovskite MgCNi3. Nature, 411, 54-56. https://doi.org/10.1038/35075014</mixed-citation></ref><ref id="hanspub.19539-ref8"><label>8</label><mixed-citation publication-type="other" xlink:type="simple">Uehara, M., Uehara, A., Kozawa, K., et al. (2009) New Anti-Perovskite-Type Superconductor ZnNyNi3. Journal of the Physical Society of Japan, 78, No. 3.</mixed-citation></ref><ref id="hanspub.19539-ref9"><label>9</label><mixed-citation publication-type="other" xlink:type="simple">Ohishi, K., Ito, T.U., Higemoto, W., et al. (2010) Quasiparticle Excitations in Newly Discovered Antiperovskite Superconductor ZnNNi3. Physica C Superconductivity, 470, S705-S706.</mixed-citation></ref><ref id="hanspub.19539-ref10"><label>10</label><mixed-citation publication-type="other" xlink:type="simple">Shein, I.R., Bannikov, V.V. and Ivanovskii, A.L. (2008) Electronic and Elastic Properties of New Nitrogen-Containing Perovskite-Like Superconductor ZnNNi3.</mixed-citation></ref><ref id="hanspub.19539-ref11"><label>11</label><mixed-citation publication-type="other" xlink:type="simple">Okoye, C.M.I. (2010) Structural, Elastic and Electronic Properties of New Antiperovskite-Type Superconductor ZnNNi3 from First-Principles. Physica B: Condensed Matter, 405, 1562-1570.</mixed-citation></ref><ref id="hanspub.19539-ref12"><label>12</label><mixed-citation publication-type="other" xlink:type="simple">Xu, Y., Gao, F., Hao, X., et al. (2010) Electronic Structure and Magnetism in Superconductor ZnNNi3: A Comparative Study with ZnCNi3 and ZnNi3. Computational Materials Science, 50, 737-741.  
https://doi.org/10.1016/j.commatsci.2010.10.004</mixed-citation></ref><ref id="hanspub.19539-ref13"><label>13</label><mixed-citation publication-type="other" xlink:type="simple">Shein, I.R., Bannikov, V.V. and Ivanovskii, A.L. (2010) Elastic and Electronic Properties of the New Perovskite-Like Superconductor ZnNNi3, in Comparison with MgCNi3. Physica Status Solidi, 247, 72-76.  
https://doi.org/10.1002/pssb.200945216</mixed-citation></ref><ref id="hanspub.19539-ref14"><label>14</label><mixed-citation publication-type="other" xlink:type="simple">Bannikov, V.V., Shein, I.R. and Ivanovskii, A.L. (2010) Elastic Properties of Antiperovskite-Type Ni-Rich Nitrides MNNi3, (M=Zn, Cd, Mg, Al, Ga, In, Sn, Sb, Pd, Cu, Ag and Pt) as Predicted from First-Principles Calculations. Physica B: Condensed Matter, 405, 4615-4619.</mixed-citation></ref><ref id="hanspub.19539-ref15"><label>15</label><mixed-citation publication-type="other" xlink:type="simple">Li, C., Chen, W.G., Wang, F., et al. (2009) First-Principles Investigation of Mechanical and Electronic Properties of MNNi3 (M=Zn, Mg, or Cd). Journal of Applied Physics, 105, No. 12. https://doi.org/10.1063/1.3156641</mixed-citation></ref><ref id="hanspub.19539-ref16"><label>16</label><mixed-citation publication-type="other" xlink:type="simple">Uehara, M., Uehara, A., Kozawa, K., et al. (2010) New Antiperovskite Superconductor ZnNNi3, and Related Compounds CdNNi3, and InNNi3. Physica C Superconductivity, 470, S688-S690.  
https://doi.org/10.1016/j.physc.2009.11.131</mixed-citation></ref><ref id="hanspub.19539-ref17"><label>17</label><mixed-citation publication-type="other" xlink:type="simple">Cao, W.H., He, B., Liao, C.Z., et al. (2010) Preparation and Properties of Antiperovskite-Type Nitrides: InNNi3, and InNCo3. ChemInform, 182, 3353-3357.</mixed-citation></ref><ref id="hanspub.19539-ref18"><label>18</label><mixed-citation publication-type="other" xlink:type="simple">Hou, Z.F. (2010) Elastic Properties and Electronic Structures of Antiperovskite-Type InNCo3, and InNNi3. Solid State Communications, 150, 1874-1879. https://doi.org/10.1016/j.ssc.2010.07.047</mixed-citation></ref><ref id="hanspub.19539-ref19"><label>19</label><mixed-citation publication-type="other" xlink:type="simple">Singer, P.M., Imai, T., He, T., et al. (2010) C13, NMR Investigation of the Super-conductor MgCNi3, up to 800 K. Physical Review Letters, 87, 257601. https://doi.org/10.1103/PhysRevLett.87.257601</mixed-citation></ref><ref id="hanspub.19539-ref20"><label>20</label><mixed-citation publication-type="other" xlink:type="simple">Bannikov, V.V., Shein, I.R. and Ivanovskii, A.L. (2010) Structural, Elastic and Electronic Properties of New Antiperovskite-Like Ternary Nitrides AlNNi3, GaNNi3, and InNNi3, as Predicted from First Principles. Computational Materials Science, 49, 457-461. https://doi.org/10.1016/j.commatsci.2010.05.036</mixed-citation></ref></ref-list></back></article>